Material Notes:
Features: High Elastic RecoveryInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
5 seconds; ASTM D2240
Tensile Strength at Break 11.4 MPa
1650 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
100% Modulus 0.00655 GPa
0.950 ksi
ASTM D412
Tear Strength 56.0 kN/m
320 pli
Die C; ASTM D624
Compression Set 36 %

@Temperature -5.00 °C,
Time 79200 sec
36 %

@Temperature 23.0 °F,
Time 22.0 hour
Method B; ASTM D395
50 %

@Temperature 21.1 °C,
Time 79200 sec
50 %

@Temperature 70.0 °F,
Time 22.0 hour
Method B; ASTM D395
58 %

@Temperature 37.8 °C,
Time 79200 sec
58 %

@Temperature 100 °F,
Time 22.0 hour
Method B; ASTM D395