Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 15
15
5 seconds; ASTM D2240
Tensile Strength, Yield 1.65 MPa
240 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
100% Modulus 0.000517 GPa
0.0750 ksi
ASTM D412
Tear Strength 7.01 kN/m
40.0 pli
ASTM D624
Compression Set 10 %
10 %
23°C, 22 hr.; ASTM D395, Method B
22 %
22 %
70°C, 22 hr.; ASTM D395, Method B
54 %
54 %
100°C, 22 hr.; ASTM D395, Method B
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746