Teknor Apex Terraloy™ MB 18003A Thermoplastic Starch + HIPS

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Teknor Apex Company
Trade Name Terraloy™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Terraloy™ MB 18003A Thermoplastic Starch + HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: Terraloy™ MB-18003A is a Thermoplastic Starch/HIPS masterbatch that contains up to 30% of TPS renewable content. High Impact PS Melt Index for the masterbatch is 9.8. This compound is intended for injection molding. Recommended letdown ration with PS is 1:1 Processing Method: Injection Molding Forms: Pellets Additional Information: Biobased Content: < 50.0Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238