Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP
Manufacturer Teknor Apex Company
Trade Name Terraloy™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: Terraloy™ BP-20001A is a Thermoplastic Starch/Biodegradable Copolyester ready-to-process compound that contains up to 40% of TPS renewable content and is 100% biodegradable. This compound is for blown film applications as well as injection molded parts. Processing Method: Blown Film; Injection Molding Forms: Pellets Additional Information: Biobased Content: < 40.0Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Oxygen Transmission Rate 404 cc/m²/day
26.0 cc/100 in²/day
ASTM D1922
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 520 %
520 %
ASTM D882
Film Elongation at Break, TD 500 %
500 %
ASTM D882
Elmendorf Tear Strength MD 300 g
300 g
ASTM D1922
Elmendorf Tear Strength TD 380 g
380 g
ASTM D1922
Dart Drop Test 290 g
0.639 lb
ASTM D1709
Film Tensile Strength at Break, MD 26.0 MPa
3770 psi
ASTM D882
Film Tensile Strength at Break, TD 20.3 MPa
2940 psi
ASTM D882