Material Notes:
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. TPV offers a lower compression set and therefore superior sealing properties. Extrusion die swell is likely to be different from TPV's due to different chemistries used. A suffix denotes grades available without filler at a density of 0.89. Compounds supplied in natural color or black. Precoloring is available upon request.Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Melt Flow 1.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
ASTM D2240
Tensile Strength 7.826 MPa
1135 psi
ASTM D412
Elongation at Break 935 %
935 %
ASTM D412
Compression Set 22 %

@Temperature 22.8 °C,
Time 79200 sec
22 %

@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395B
42 %

@Temperature 70.0 °C,
Time 79200 sec
42 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395B