Material Notes:
Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection molded siding panels, pool products, transportation parts, various home products as well as other applications requiring higher rigidity, lower shrinkage and lower coefficient of linear thermal expansion than natural polyolefins. These compounds can be tailored to specific needs and are available pre-colored or natural. Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Melt Flow 12.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
10 seconds; ASTM D2240
Tensile Strength at Break 21.4 MPa
3100 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256