Teknor Apex Sinvicomp SFR 5800C2 Polyvinyl Chloride, Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp SFR 5800C2 Polyvinyl Chloride, Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Asia Pacific Features: Foamable Uses: Profiles; Foam Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C

@Time >=3600 sec
374 °F

@Time >=1.00 hour
Congo Red; ASTM D2115-92
Vicat Softening Point 75.0 °C
167 °F
ASTM D1525