Teknor Apex Sinvicomp DBS 8602 Polyvinyl Chloride, Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp DBS 8602 Polyvinyl Chloride, Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Asia Pacific Features: Good Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
9.8 in/min; ASTM D638
Elongation at Break 160 %
160 %
9.8 in/min; ASTM D638
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C

@Time >=3600 sec
374 °F

@Time >=1.00 hour
Congo Red; BS 2782
Vicat Softening Point 96.1 °C
205 °F
ASTM D1525