Teknor Apex Sinpolene FRF2074 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Teknor Apex Company
Trade Name Sinpolene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinpolene FRF2074 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.938 g/cc
0.938 g/cc
ASTM D792
Linear Mold Shrinkage 0.00013 cm/cm
0.00013 in/in
ASTM D955
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Izod Impact, Notched 0.251 J/cm

@Temperature 22.8 °C
0.470 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
Unannealed; ASTM D648
Vicat Softening Point 154 °C
309 °F
Loading 1 (10N); ASTM D1525
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in