Teknor Apex Sinelec CCB1861 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Teknor Apex Company
Trade Name Sinelec
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinelec CCB1861 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Films; Packaging Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Melt Flow 3.00 g/10 min

@Load 10.0 kg,
Temperature 190 °C
3.00 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
<= 600 %
<= 600 %
Across Flow; ASTM D638
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
ASTM D257
Surface Resistance 1e+05
1e+05
ASTM D257