Teknor Apex MONPRENE® MP 2820M Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name MONPRENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex MONPRENE® MP 2820M Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
ASTM D792
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 20
20
ASTM D2240
Tensile Strength, Yield 4.83 MPa
700 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
300% Modulus 0.000621 GPa
0.0900 ksi
ASTM D412
Users viewing this material also viewed the following: