Teknor Apex HFFR 2005PC Polyolefin, Halogen Free

Category Polymer , Thermoplastic , Polyolefin , Polyolefin, Wire/Cable Grade
Manufacturer Teknor Apex Company
Trade Name HFFR
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex HFFR 2005PC Polyolefin, Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable JacketingAgency Ratings: IEC Unspecified Rating; ICEA Unspecified Rating; UL QMTT2 .E200337 Processing Method: Extrusion Forms: Pellets Additional Information: Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 100°C: 86% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 100°C: 106% Cone Calorimeter at 50 kW/m2, Peak Heat Release Rate: 266 kW/m2 Cone Calorimeter at 50 kW/m2, Total Heat Released: 195 MJ/m2 Cone Calorimeter at 50 kW/m2, Peak Smoke: 2.0 1/m Cone Calorimeter at 50 kW/m2, Time to Sustained Ignition: 106 secInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Melt Flow 15.0 g/10 min

@Load 10.0 kg,
Temperature 190 °C
15.0 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
10 seconds; ASTM D2240
Tensile Strength at Break 13.8 MPa
2000 psi
ASTM D638
Elongation at Break 270 %
270 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -50.0 °C
-58.0 °F
ASTM D746
Oxygen Index 34 %
34 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 6.40e+14 ohm-cm
6.40e+14 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 1000 Hz
3.4

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque