Teknor Apex Flexalloy® 3500-55 Polyvinyl Chloride Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC)
Manufacturer Teknor Apex Company
Trade Name Flexalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Flexalloy® 3500-55 Polyvinyl Chloride Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
15 seconds; ASTM D2240
Tensile Strength, Yield 3.79 MPa
550 psi
100%; ASTM D412
11.0 MPa
1600 psi
ASTM D412
Elongation at Break 380 %
380 %
ASTM D412
Tear Strength, Total 688.2 N
154.7 lb (f)
Die C; ASTM D1004
Compression Set 14 %
14 %
73°F, 22 hr.; ASTM D395
56 %
56 %
158°F, 22 hr.; ASTM D395
61 %
61 %
212°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -50.0 °C
-58.0 °F
ASTM D746