Teknor Apex Fireguard® 910-FOB-NL1 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Fireguard®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Fireguard® 910-FOB-NL1 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: Plenum Cable Jacketing; Wire and Cable Applications Agency Ratings: UL QMTT2 .E200337 Forms: Pellets Additional Information: Dynamic Heat Stability at 205°C, 100 rpm, 72 gr. #5 Bowl (Minutes to Decomposition): 57 Kayness ACR at 350°F, 1000 sec-1: 290 Pa-s Cone Calorimeter at 75 kW/m2, Peak Heat Release Rate: 111 kW/m2 Average Heat Release Rate: 60 kW/m2 Total Heat Released: 77 MJ/m2 Average Heat of Combustion: 13.5 MJ/kg Average Specification Extinction Area: 325 m2/kg Peak Smoke: 2.3 1/mInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 83
83
10 seconds; ASTM D2240
Tensile Strength at Break 17.2 MPa
2500 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Continuous Use; ASTM D794
Brittleness Temperature -8.00 °C
17.6 °F
ASTM D746
Oxygen Index 42 %
42 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.59

@Frequency 1.00e+6 Hz
3.59

@Frequency 1.00e+6 Hz
ASTM D150
4.65

@Frequency 1000 Hz
4.65

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 30.3 kV/mm
770 kV/in
ASTM D149
Dissipation Factor 0.035

@Frequency 1.00e+6 Hz
0.035

@Frequency 1.00e+6 Hz
ASTM D150
0.083

@Frequency 1000 Hz
0.083

@Frequency 1000 Hz
ASTM D150