Teknor Apex ELEXAR® EL 8431 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name ELEXAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex ELEXAR® EL 8431 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
ASTM D2240
Tensile Strength, Yield 19.8 MPa
2870 psi
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous; UL-1581
Brittleness Temperature -100 °C
-148 °F
ASTM D746
Oxygen Index 18 %
18 %
ASTM D2863