Material Notes:
Notes: Sunlight Resistant; Temperature Rating: 105°C Processing Method: Extrusion; Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
Tensile Strength 16.7 MPa
2420 psi
Elongation at Break 650 %
650 %
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746
Flammability, UL94 HB
HB
Oxygen Index 18 %
18 %
ASTM D2863