Teknor Apex Chemlon® 109-33 GH Nylon 66, 33% Glass Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Teknor Apex Company
Trade Name Chemlon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Chemlon® 109-33 GH Nylon 66, 33% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: High-Impact; Reinforced with 33% Glass Fibers; Highly toughened compound exhibiting strength and rigidity Features: Good Creep Resistance; Good Stiffness; High Strength; Good Impact Resistance; Good Toughness; Good Processability; Heat Stabilized Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Water Absorption 0.80 %
0.80 %
24 hr; ASTM D750
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 138 MPa
20000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 203 MPa
29500 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Temperature 22.8 °C
3.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 246 °C
475 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 293 °C
560 °F
Middle Barrel Temperature 282 °C
540 °F
Front Barrel Temperature 277 °C
530 °F
Nozzle Temperature 277 °C
530 °F
Mold Temperature 60.0 - 93.3 °C
140 - 200 °F
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
Injection Pressure 34.5 - 138 MPa
5000 - 20000 psi
Screw Speed 60 - 120 rpm
60 - 120 rpm
Descriptive Properties Value Comments
Appearance Black; Natural Color
Suggested Moisture, max 0.2