Teknor Apex Beetle® MD82 Nylon 6, Non-halogenated, Dry

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Teknor Apex Company
Trade Name Beetle®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Beetle® MD82 Nylon 6, Non-halogenated, Dry.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: MD82 is a UL recognized, V-0 rated halogen and phosphorus-free flame retarded, heat stabilized, unreinforced injection molding grade of nylon 6; U.L. 94 V-O at 0.63mm. Colorable Features: Flame Retardant; Halogen free; Low (to no) Phosphorus Content; Good Colorability; Heat Stabilized Processing Method: Injection MoldingForms: Pellets Additive: Heat Stabilizer Injection Notes: No drying is necessary unless the material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure: High; Injection Rate: FastInformation Provided by Teknor Apex
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 0.630 mm
V-0

@Thickness 0.0248 in
Processing Properties Metric English Comments
Rear Barrel Temperature 240 - 260 °C
464 - 500 °F
Middle Barrel Temperature 240 - 260 °C
464 - 500 °F
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Melt Temperature <= 300 °C
<= 572 °F
Processing Temperature
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 hour
2 hour
Screw Speed 50 - 200 rpm
50 - 200 rpm