Teknor Apex Beetle® A82 Nylon 66, Non-Halogenated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant
Manufacturer Teknor Apex Company
Trade Name Beetle®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Beetle® A82 Nylon 66, Non-Halogenated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: A82 is a UL recognized. V-0 rated halogen and phosphorus-free flame retarded, heat stabilized, unreinforced injection molding grade of nylon 66. Features: Flame Retardant; Heat Stabilized; Halogen Free; Low (to no) phosphorus contentProcessing Method: Injection Molding Forms: Pellets Injection Notes: Drying is necessary if material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure; High; Injection Rate: FastInformation Provided by Teknor Apex
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 0.569 mm
V-0

@Thickness 0.0224 in
Processing Properties Metric English Comments
Rear Barrel Temperature 270 - 290 °C
518 - 554 °F
Middle Barrel Temperature 270 - 290 °C
518 - 554 °F
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Melt Temperature <= 300 °C
<= 572 °F
Processing Temperature
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 hour
2 hour
Screw Speed 50 - 200 rpm
50 - 200 rpm