Teknor Apex APEX® 77-W115-B Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 77-W115-B Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 105°C General Purpose; RoHS Compliant Uses: Connects; Grommets; Plugs; Strain ReliefsForms: Pellets Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: Temperature Rating: 105°CInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
15 seconds; ASTM D2240
Tensile Strength at Break 17.2 MPa
2500 psi
ASTM D638
Elongation at Break 360 %
360 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -15.0 °C
5.00 °F
ASTM D746
Flammability, UL94 V-2

@Thickness 0.800 mm
V-2

@Thickness 0.0315 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 29 %
29 %
ASTM D2863
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V

@Thickness 3.00 mm
>= 600 V

@Thickness 0.118 in
UL 746
Hot Wire Ignition, HWI 60 - 120 sec

@Thickness 3.00 mm
60 - 120 sec

@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI 60 - 120 arcs

@Thickness 3.00 mm
60 - 120 arcs

@Thickness 0.118 in
UL 746
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Processing Temperature
Descriptive Properties Value Comments
Appearance Opaque