Material Notes:
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: Temperature Rating: 105°CInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
15 seconds; ASTM D2240
Tensile Strength at Break 12.6 MPa
1830 psi
ASTM D638
Elongation at Break 420 %
420 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
UL RTI, Electrical 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
UL RTI, Mechanical with Impact 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
UL RTI, Mechanical without Impact 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Melt Temperature 174 °C
345 °F
Processing Temperature
Descriptive Properties Value Comments
Appearance Opaque