Material Notes:
Notes: 105°C Insulation; RoHS Compliant Features: High Heat Resistance Uses: Wire and Cable Applications; Flexible Cord Insulation; Wire JacketingForms: Pellets Wire Types: SPT-1; SPT-2; SPT-3 Agency Ratings: UL 62 Processing Method: Extrusion Additional Information: Temperature Rating: 105°C Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 136°C: 77% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 136°C: 106%Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Melt Flow 0.500 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.500 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
15 seconds; ASTM D2240
Tensile Strength at Break 18.6 MPa
2700 psi
ASTM D638
Elongation at Break 340 %
340 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -38.0 °C
-36.4 °F
ASTM D746
Oxygen Index 23 %
23 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Descriptive Properties Value Comments
Appearance Clear/Transparent