Teknor Apex APEX® 65009 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 65009 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
15 seconds; ASTM D2240
Tensile Strength at Break 16.9 MPa
2450 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Continuous Use; ASTM D794
Brittleness Temperature -23.0 °C
-9.40 °F
ASTM D746
Oxygen Index 38 %
38 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 4.10e+13 ohm-cm
4.10e+13 ohm-cm
ASTM D257
Descriptive Properties Value Comments
Appearance Opaque