Teknor Apex APEX® 4157 Polyvinyl Chloride Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 4157 Polyvinyl Chloride Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: Non-Migrating; Sunlight Resistant, Tray Cable Jacket Temperature Rating: 105°CInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
ASTM D2240
Tensile Strength 16.5 MPa
2400 psi
ASTM D638
Elongation at Break 425 %
425 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -33.0 °C
-27.4 °F
ASTM D746
Oxygen Index 31 %
31 %
ASTM D2863