Teknor Apex APEX® 01-A0402C-112 Polyvinyl Chloride, Semi-Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 01-A0402C-112 Polyvinyl Chloride, Semi-Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 105°C Insulation; RoHS Compliant Uses: Automotive Electronics; InsulationWire Types: TWP Agency Ratings: SAE J1128 Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 88
88
10 seconds; ASTM D2240
Tensile Strength at Break 23.6 MPa
3420 psi
ASTM D638
Elongation at Break 290 %
290 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -27.0 °C
-16.6 °F
ASTM D746
Oxygen Index 26 %
26 %
ASTM D2863
Descriptive Properties Value Comments
Appearance Opaque