Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveUL File Number: E157318TPCI# 1038102Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 1.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
1.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 89
89
ASTM D785
Tensile Strength, Yield 82.7 MPa
12000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 130 MPa
18900 psi
ASTM D790
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D257
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D257