Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Techmer ES
Trade Name Statiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® HIPS C BK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: ConductiveAppearance: BlackTPCI# 7576148Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
38.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm - 1e+05
1000 ohm-cm - 1e+05
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
Users viewing this material also viewed the following: