Techmer ES Statiblend® 02036 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Techmer ES
Trade Name Statiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® 02036 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Water Absorption 0.010 %

@Time 86400 sec
0.010 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.017 cm/cm

@Thickness 3.17 mm
0.017 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 32.4 MPa
4700 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 1.14 GPa
165 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.0 µm/m-°C
45.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 - 1.00e+12 ohm-cm
1.00e+8 - 1.00e+12 ohm-cm
ASTM D257
Surface Resistance 1.00e+8 - 1.00e+12 ohm
1.00e+8 - 1.00e+12 ohm
ASTM D257