Techmer ES Plastiblend® TPX-HTN-000CA

Category Polymer , Thermoplastic , Nylon , High Temperature Nylon
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® TPX-HTN-000CA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 0.65 %

@Time 86400 sec
0.65 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 128 MPa
18500 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 9.61 J/cm

@Thickness 3.17 mm
18.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
38.0 µin/in-°F
ASTM D696
Melting Point 154 °C
310 °F
Maximum Service Temperature, Inert 160 °C
320 °F
ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
Unannealed; ASTM D648