Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® PSU CR X

Category Polymer , Thermoplastic , Polysulfone (PSU) , Polysulfone, Modified
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® PSU CR X.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: TPU Impact Modifier Features: Impact ModifiedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 88.3 MPa
12800 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 110 MPa
15900 psi
ASTM D790
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm

@Thickness 3.17 mm
1.70 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Strength 21.7 kV/mm
550 kV/in
Method A (Short-Time); ASTM D149
Copyright © lookpolymers.com All Rights Reserved