Material Notes:
Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Thickness 3.17 mm
0.0070 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
7.0 g/10 min

@Load 5.00 kg,
Temperature 260 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 110 %
110 %
ASTM D638
Flexural Yield Strength 95.8 MPa
13900 psi
ASTM D790
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm
9.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 118 °C
245 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB