Material Notes:
Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 3.3 g/10 min

@Load 10.0 kg,
Temperature 260 °C
3.3 g/10 min

@Load 22.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength at Break 51.7 MPa
7500 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 84.8 MPa
12300 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
1.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
1.01 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
1.90 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
1.28 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.6 °C
168 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB