Techmer ES Plaslube® NY-1/TF/13/SI/2 Nylon 66, 13% PTFE, 2% Silicone

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, PTFE Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® NY-1/TF/13/SI/2 Nylon 66, 13% PTFE, 2% Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearings and bushings.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.9 MPa
10000 psi
ASTM D638
Flexural Yield Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648