Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plaslube® J-50/20/SI/2 Polycarbonate, 20% GFR, 2% Silicone

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® J-50/20/SI/2 Polycarbonate, 20% GFR, 2% Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.090 %
0.090 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 110 MPa
16000 psi
ASTM D638
Flexural Yield Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D790
Compressive Strength 110 MPa
16000 psi
ASTM D695
Izod Impact, Notched 1.92 J/cm

@Thickness 3.17 mm
3.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in