Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Water Absorption 0.13 %
0.13 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 138 MPa
20000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 197 MPa
28500 psi
ASTM D790
Flexural Modulus 8.34 GPa
1210 ksi
ASTM D790
Compressive Strength 124 MPa
18000 psi
ASTM D695
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 48.6 µm/m-°C

@Temperature 20.0 °C
27.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in