Techmer ES Luriblend® TPX-PPO/HIPS-02072 BK

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) , Polystyrene + Polyphenylene Ether + Nylon, Unreinforced
Manufacturer Techmer ES
Trade Name Luriblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® TPX-PPO/HIPS-02072 BK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and HomopolymerUL File Number: E157318Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 37.9 MPa
5500 psi
ASTM D638
Elongation at Yield 55 %
55 %
ASTM D638
Flexural Yield Strength 83.4 MPa
12100 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 2.19 J/cm

@Thickness 3.17 mm
4.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 21.4 J/cm

@Thickness 3.17 mm
40.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 97.2 °C
207 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257