Techmer ES Luriblend® PC GF30 TL15 30% Glass Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled , Polycarbonate, PTFE Filled
Manufacturer Techmer ES
Trade Name Luriblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® PC GF30 TL15 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 28.8 µm/m-°C
16.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
Unannealed; ASTM D648
Flammability, UL94 V-1
V-1