Techmer ES Luriblend® HIPS TL10 BK

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Techmer ES
Trade Name Luriblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® HIPS TL10 BK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Good Wear Resistance, Low Friction and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
8.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 35.9 MPa
5200 psi
ASTM D790
Flexural Modulus 1.59 GPa
230 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.17 mm
1.90 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Strength 18.1 kV/mm
460 kV/in
Method A (Short-Time); ASTM D149