Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® TPU GF30 30% Glass Filled

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Glass Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® TPU GF30 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ASTM D792
Water Absorption 0.25 %

@Time 86400 sec
0.25 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 65
65
ASTM D785
Tensile Strength, Yield 56.5 MPa
8200 psi
ASTM D638
Elongation at Yield 25 %
25 %
ASTM D638
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched 5.87 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 45.0 µm/m-°C
25.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 171 °C
340 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Strength 15.7 kV/mm
400 kV/in
Method A (Short-Time); ASTM D149