Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PBT 1226

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PBT 1226.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.020 cm/cm

@Thickness 3.17 mm
0.020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 137 µm/m-°C
76.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+15 ohm-cm
3.00e+15 ohm-cm
ASTM D257
Dielectric Strength 16.1 kV/mm
410 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: