Techmer ES HiFill® PA6 GF/M25 HS L BK 25% Glass/Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced , Nylon 6, Heat Stabilized
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6 GF/M25 HS L BK 25% Glass/Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackTPCI# 7151102Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Thickness 3.17 mm
0.0090 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Izod Impact, Notched 0.187 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
0.350 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
0.427 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.800 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 196 °C
385 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Strength 15.7 kV/mm
400 kV/in
Method A (Short-Time); ASTM D149