Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® HDPE GF60 60% Glass Filled

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Glass fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® HDPE GF60 60% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D792
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 46.9 MPa
6800 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 91.0 MPa
13200 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm

@Thickness 3.17 mm
2.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 µm/m-°C
11.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
290 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
Unannealed; ASTM D648