Material Notes:
Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: Natural ColorInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Water Absorption 0.040 %

@Time 86400 sec
0.040 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Yield 45 %
45 %
ASTM D638
Flexural Modulus 1.34 GPa
195 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
205 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C
155 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149