Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill FR® PBT GF30 CF10 FR 30/10% Glass/Carbon Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled , Polybutylene Terephthalate (PBT), Carbon Fiber Filled , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® PBT GF30 CF10 FR 30/10% Glass/Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber, 30/10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength 128 MPa
18500 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 200 MPa
29000 psi
ASTM D790
Flexural Modulus 10.7 GPa
1550 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 µm/m-°C
11.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0