Material Notes:
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 0.95 %

@Time 86400 sec
0.95 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm
2.30 ft-lb/in

@Thickness 0.125 in
ASTM D256