Techmer ES HiFill FR® HDPE FR-HB

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® HDPE FR-HB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Strength 35.2 MPa
5100 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB