Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill FR® HDPE 8904 FR UV GY

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® HDPE 8904 FR UV GY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceAppearance: GrayInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Flexural Modulus 1.03 GPa
150 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0