Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrafil® PC-50/EC/VO Polycarbonate, Conductive Carbon Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Conductive
Manufacturer Techmer ES
Trade Name Electrafil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrafil® PC-50/EC/VO Polycarbonate, Conductive Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conductive Carbon, Powder Modified with Flame Retardant
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.8 MPa
8100 psi
ASTM D638
Flexural Yield Strength 84.1 MPa
12200 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1000 - 1.00e+6 ohm
1000 - 1.00e+6 ohm
ASTM D4496