Techmer ES Electrafil® PC-50/EC Polycarbonate, Conductive Carbon Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Conductive
Manufacturer Techmer ES
Trade Name Electrafil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrafil® PC-50/EC Polycarbonate, Conductive Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conductive Carbon, Powder Modified
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 10.7 J/cm

@Thickness 3.17 mm
20.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1000 - 10000 ohm
1000 - 10000 ohm
ASTM D4496
Static Decay 0.050 sec
0.050 sec