Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrablend® PA6/6 C14 BK 14% Carbon Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Carbon Fiber Filled , Nylon 66, Conductive
Manufacturer Techmer ES
Trade Name Electrablend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® PA6/6 C14 BK 14% Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 152 MPa
22000 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Flexural Strength 255 MPa
37000 psi
ASTM D790
Flexural Modulus 10.7 GPa
1550 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.2 µm/m-°C
39.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 259 °C
498 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
ASTM D257
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
Users viewing this material also viewed the following: